SCR honeycomb ceramics mainly have the following functions:
project | |||||
Thermal shock resistance | Keep at650 ºC for 30 minutes, quickly remove and cool at room temperature for 30 minutes. Repeat this process continuously for 3 times | muffle furnace | |||
compressive strength | A-axis | >=5Mpa | Compression strength machine | ||
B-axis | >=1.4Mpa | ||||
Thermal expansion coefficient (room temperature -800 ºC) | <=1.0 | Thermal expansion coefficient meter | |||
Water absorption rate | 22%-28% | Electronic scale | |||
Content of main crystal phase in cordierite | >=90% | XRD | |||
chemical composition | AL203 | 35.4±1.5 | |||
Mg0 | 13.5±1.5 | ||||
Si02 | 49.7±1.5 | ||||